The first issue of the topic series “Superalloys” contains articles published by Trans Tech Publications in 2017 year. The volume entitled as "Ni-Based Superalloys" provides the readers with a wide range of scientific research results and engineering solutions in the field of development, a study of properties and processing technologies of nickel-based superalloys. We hope this collection will be useful and interesting to a broad audience of researchers and engineers from the area of machinery.

Les mer
<p>Aggregated Book</p>
  • Preface
  • Chapter 1: Microstructure of Alloys
  • The 3D Imaging and Metrology of Microstructural Elements in Innovative Materials for Clean Energy Systems and Aeronautics
  • Metallography Evaluation of Cast and Wrought Ni-Base Superalloys
  • Effect of Long-Term Aging on Microstructural Restoration in Cast Nickel Base Superalloy, GTD-111
  • Effect of Temperature Dropping during Solution Treatment in Rejuvenation Heat Treatment and its Long-Term Heating Simulation on Microstructures of Nickel Base Alloy, Udimet 520
  • Long-Term Gamma Prime Phase Stability after Various Heat Treatment Conditions with Temperature Dropping during Solution Treatment in Cast Nickel Base Superalloy, Grade Inconel-738
  • Effect of Precipitation Aging Temperatures on Reheat Treated Microstructures and its Phase Stability after Long-Term Exposure in Cast Nickel Base Superalloy, Grade Inconel 738
  • Effect of Solution Treatment Temperature on the Grain Growth Behavior of Fine Grained FGH96 Superalloy
  • Effect of Strain Hardening on Precipitation Kinetics in ATI 718Plus
  • Oxidation Behavior of a Disk Powder Metallurgy Superalloy
  • Morphology Evolution of Grain Boundary Carbides in Highly Twinned Inconel Alloy 600
  • Morphological Evolution of Carbides in DZ125 Superalloy during Heat Treatment
  • Microstructure and Property Calculation of Three Typical Second Generation Single Crystal Superalloys
  • The Precipitation Behavior of γ′ Phase in Single Crystal Ni-Based DD6 Superalloy for Turbine Blade
  • A Review of Rafting in Nickel-Based Single Crystal Superalloys
  • The Influence of γ/γ′ Morphology on the Rafting and Stress Distribution of Nickel-Based Superalloys Loaded in [0 0 1] Direction
  • Chapter 2: Mechanical Behaviour and Deformation Modelling
  • Small Ring Testing of High Temperature Materials
  • Stabilities of Microstructure and Mechanical Properties during Long-Term Aging on FGH95 Superalloy
  • Influence of Dynamic Strain Ageing and Long Term Ageing on Deformation and Fracture Behaviors of Alloy 617
  • Influences of W and Al on the Microstructure and Stress-Rupture Property of Re-Free Ni-Based Single Crystal Superalloys
  • Long Time High Temperature Stress Rupture Strength Behavior and Structure Stability Study on Ni-Base Superalloy Nimonic 80A
  • Degradation of the Strength of Grains and Grain Boundaries of Ni-Base Superalloy under Creep and Creep-Fatigue Loadings
  • Creep Processes in MAR-M247 Nickel-Base Superalloy
  • Microstructure Evolution and Stress Rupture Properties of DD6 Single Crystal Superalloy after Overheating
  • Microstructure Evolution and Creep Properties of a Single Crystal Nickel-Based Superalloy with Various Orientations
  • High Temperature Rupture Life of Nickel-Based Superalloy under Directional Solidification with High Temperature Gradient
  • Creep Behavior of a Ru-Free Nickel-Based Single Crystal Superalloy at Medium Temperatures
  • Mechanical Behaviour of Materials during Creep with Changing Loads
  • Interaction of Creep and High Cycle Fatigue of IN 713LC Superalloy
  • Failure Assessment of the First Stage High Pressure Turbine Blades
  • Fatigue Crack Initiation in Nickel-Based Superalloy MAR-M247 at High Temperature
  • Effect of Maximum Temperature on the Thermal Fatigue Behavior of Superalloy GH536
  • Characteristics of Microscopic Inclusions and their Influence on Fatigue Crack Propagation in FGH96 Superalloy
  • Initiation and Propagation Behaviors of Small Crack in a Polycrystalline Ni-Base Superalloy under Thermo-Mechanical Fatigue Loading
  • Effect of Frequency on the Fatigue Behavior of IN718 Superalloy
  • Surface Roughness Effects on the Fatigue Behavior of As-Machined Inconel718
  • Crystal Plasticity Simulations of Haynes 230, an Analysis of Single Crystal and Polycrystalline Experiments
  • Fatigue Crack Propagation in Haynes 230: A Comparison between Single and Polycrystal Crack Closure Levels
  • Fatigue Crack Growth in Flow Formed INCONEL 718
  • Chapter 3: Solidification and Processing
  • Effect of Hot Isostatic Pressing on Microstructures and Mechanical Properties of IN738LC Superalloy
  • Effects of HIP Process on the Microstructure and Mechanical Properties of a Cast Superalloy
  • Microstructure Study of Nickel-Based Superalloys after Deep Cold Rolling
  • Analysis of Deformation and Internal Defect in Flat-Wedge Cross-Wedge Rolling of GH4169 Superalloy
  • A Novel Unified Dislocation-Density Based Model for Hot Deformation Behavior of a Nickel-Based Superalloy
  • Hot Deformation Behavior of AA-FGH720Li Superalloy
  • The Addition of Zr in Nickel-Based Inconel 718 Superalloy to Prevent Hot Cracks Propagation
  • Precision Casting of GTD222 Component with Complex Thin-Wall Structure
  • Early Instability Phenomena of IN792 DS Superalloy
  • Simulation and Experimental Studies on Grain Selection Behavior of DD5 Single Crystal Superalloy
  • Microstructures of Low Angle Boundaries of a Third Generation Single Crystal Superalloy DD9
  • The Effect of Process Parameters in Interdendritic-Melt Solidification Control Technique on the Microstructure and Properties of a Ni-Base Superalloy
  • Effect of Low-Angle Boundary on Microstructure and Stress Rupture Property of a Third Generation Single Crystal Superalloy DD10
  • Study on the Formation of Stray Grains during Directional Solidification of Nickel-Based Superalloys
  • Chapter 4: Welding and Laser Deposition
  • Thermal Cycle Simulation of Welding Process in INC 738 LC Superalloy
  • Welding of IN792 DS Superalloy by High Energy Density Techniques
  • IN792 DS Superalloy: Optimization of EB Welding and Post-Welding Heat Treatments
  • The Microstructure of Inconel Alloys Used for Repair Welding
  • Linear Friction Welding of IN718 to Ti6Al4V
  • Measurement of Residual Stresses in Linear Friction Welded In-Service Inconel 718 Superalloy
  • Investigation of Impact Behavior of TIG Welded Inconel 718 at Aircraft Engine Operating Temperatures
  • Crack Growth Studies in a Welded Ni-Base Superalloy
  • Evaluation on the Corrosion and Wear Resistance of Welding Zone Welded with Plasma Transferred Arc Welding Method
  • Structure Formation in Ni Superalloys during High-Speed Direct Laser Deposition
  • Preliminary Experimental Study of Laser Cladding Repair on Directionally Solidified Blades
  • Effect of Build Orientation and Post Processing of a Direct Laser Deposited Nickel Superalloy as Determined by the Small Punch Creep Test
  • A Study on the Microstructural Characterization of René 142 Deposited Atop René 125 Processed through Scanning Laser Epitaxy
  • Brazing Inconel 600 Using the VZ-2150 Filler for Plate Heat Exchanger
  • Brazing Inconel 600 to Manufacture the Plate Heat Exchanger
  • Chapter 5: Thermal Barrier Coatings
  • Phase Stability, Structure and Thermodynamics of Modified Ni- and Fe-Aluminides
  • Durability of Amorphous and Crystalline BMAS Thermal Barrier Coatings Produced by Plasma Spraying
  • Formation of Thermally Sprayed Coatings on Grid-Like Structure Substrate
  • Research on the Stability of Thermal Barrier Coatings under Thermal Cyclic Loading
  • Interdiffusion Databanks of γ, γ′ and β Phases in NiAl-Based Ternary Systems
  • Cyclic Oxidation Performance of Si-Aluminide/MCrAlY Coating on Ni-Base GTD-111 Superalloy
  • The Study of High Temperature Oxidation Performance of Thermal Barrier Coatings Prepared by Plasma Spraying and Laser Remelting
  • Diffusion-Controlled Growth and Microstructural Evolution of Aluminide Coatings on Superalloys and Steel
  • Sintering Study of NiCrAlY
  • Effect of Double Electron Beam Remelting on Microstructure of HVOF and CGDS Bond Coat
  • EBSD Analysis and Assessment of Porosity in Thermal Barrier Coatings Produced by Axial Suspension Plasma Spraying (ASPS)
  • Development of the Advanced TBC for High Efficiency Gas Turbine
  • Material and Mechanical Aspects of CMAS Damage Progression on Thermal Barrier Coatings and its Non-Destructive Detection
  • Failure Mechanism of Yttria Stabilized Zirconia Atmospheric Plasma Sprayed Thermal Barrier Coatings Subjected to Calcia-Magnesia-Alumino-Silicate Environmental Attack
  • Degradation of YSZ/EUCOR TBC Coating System during High Temperature Low Cycle Fatigue Tests
  • The Application of the Small Punch Tensile Test to Evaluate the Ductile to Brittle Transition of a Thermally Sprayed CoNiCrAlY Coating
  • Measurement of Young’s Modulus of Thermal Barrier Coatings by Suspended Coupled Flexural Resonance Method
  • The High Temperature Creep Properties of a Thermally Sprayed CoNiCrAlY Coating via Small Punch Creep Testing
  • Investigation on Fracture Toughness of Coating/Substrate Interface - Case Study: Thermally Sprayed Nickel Based Superalloy on Variety of Substrates
  • Thermomechanical and Thermal Gradient Mechanical Fatigue Lifetime of Thermal Barrier Coating Systems
  • Thermo-Mechanical and Low Cycle Fatigue Failure Behavior Relevant to Temperature Regime in a TBCed Superalloy Specimen
  • Chapter 6: Machining Processes
  • Specific Cutting Force in Turning of Sintered Nickel Alloy
  • Manufacturing of Axisymmetric Components out of Superalloys and Hard-to-Deform Steels by Roll Forming
  • Influence of Coolant Application Direction on the Cutting Performance of Ceramic Tool in High-Speed Air-Jet-Assisted Machining of Inconel 718
  • Experimental Study on the Relationship of Discharge Parameters with Crack Arrest Effects in Inconel 625 Alloy by Electropulsing Treatment
  • Machinability of Inconel 625 Aerospace Material Using Cryogenically Treated WEDM
  • Experimental Study on Electro-Discharge Machining of Nickel-Based Superalloy
Les mer

Produktdetaljer

ISBN
9783035711615
Publisert
2020-07-28
Utgiver
Trans Tech Publications Ltd; Trans Tech Publications Ltd
Vekt
1340 gr
Høyde
240 mm
Bredde
170 mm
Dybde
36 mm
Aldersnivå
P, 06
Språk
Product language
Engelsk
Format
Product format
Heftet
Antall sider
720